Shipping & quality / Bevel checks
SPC bevel defects: names, causes and where to check
A painted SPC bevel is milled into the core, then lacquered. Name each bevel defect, tell it apart from a click fault and check it on assembled boards.
Short answer
Specify the bevel by type, angle, depth and colour on a drawing tied to the approved sample, then judge it on assembled boards. A micro bevel is milled into the wear layer, a painted bevel is milled deeper and lacquered, and a pressed bevel pushes the decor down. Most bevel faults start at the milling tool or the lacquer unit; a gap or step at the joint is a locking or squareness fault.
Unilin describes the lacquered bevel as milled through the top layer into part of the core, then finished with coloured lacquer. Wherever the lacquer misses, the core shows.
ISO 24337:2019 measures openings and height differences between assembled elements; ISO 24342:2024 measures side length, edge straightness and squareness of resilient planks. Neither standard names the bevel, so its limits go in your PO.
The data sheet of one bevel coating unit lists three applicator discs covering bevel angles from 5° to 45°, set by a central adjustment. A new angle or tool after approval is a new edge, and it needs a new sample.
A bevel is the edge a customer sees on every board in the room, and the one property most specifications cover with a single word. “4V bevel” does not say how the edge is made, how deep it goes or what colour it should be. The factory fills those gaps, and the inspector has nothing to fail against.
What kinds of bevel are on SPC, and how is each made?
Four edge types reach the market, and each is made at a different point in production. Micro and painted bevels are milled on the profiling line; a pressed bevel is formed by pressing the decor down rather than cutting it; a square edge has none. Sellers’ names vary (V-groove, 4V, painted bevel), and the method decides which defects you can get, so the spec names the method and the dimensions.
The table sets out each type as the technology licensor Unilin and one coating-equipment maker describe it, read in November 2026, and what the spec must fix for each.
| Edge type | How it is made | What the edge shows | Fix in the spec |
|---|---|---|---|
| Micro bevel | Milled at a shallow angle into the wear layer | Wear layer and print, cut at an angle | Angle, depth, sides (2 or 4) |
| Painted (lacquered) bevel | Milled through the top layer into part of the core, then lacquered | Lacquer over core | Angle, depth, lacquer colour and gloss, sides |
| Pressed bevel | Decor and texture pressed down into the bevel | Decor running to the bottom of the bevel | Depth, width, method and licence |
| No bevel (square edge) | No chamfer milled | Surface meets surface | Square edge stated, so it is not added later |
Unilin’s description of the micro bevel is milling away part of the wear layer at a shallow angle, so the deeper it is cut, the less wear layer is left at the edge. That ties the bevel to the wear-layer figure you contracted, which our guide on checking an SPC wear layer sets out. Unilin also notes that vinyl floors with micro bevels often show shiny edges, most visibly on light designs; that gloss line is a bevel property and belongs in the spec.
Unilin’s lacquered bevel can be finished in a shade matching or contrasting with the decor. On the line, the lacquer goes on straight after milling. Kraft Group lists chamfer painting as part of its profiling lines for laminate and for LVT, and Schiele’s TransferDisc data sheet describes a unit that lacquers only the bevel, not the profile, at line speeds up to 160 m/min, with a central adjustment for different bevel angles.
The pressed bevel pushes the decor layer and texture down so they continue to the deepest point of the bevel. Unilin describes the method as patented and says pressed bevels on resilient flooring are often long and flat, with misaligned bevels and high scrap rates among the production problems it was designed to solve. Misalignment is the defect to name for this type.
Which bevel defects should the spec name?
Name each defect in the spec so the inspector can count it. Each one traces back to the milling tool, the lacquer unit, the press or the film lot, and the cause tells you what to ask the factory to change. A defect without a name in the spec ends up as a remark in the report, and a remark fails nothing.
The names below are our working terms. The cause column follows from how each bevel is made, as described above.
| Defect | What you see | Bevel types | Likely source |
|---|---|---|---|
| Paint overspill | Lacquer on the face beside the bevel, or on the click profile | Painted | Lacquer unit set-up, worn applicator, wrong angle setting |
| Missed or thin paint (exposed core) | Core colour visible in the groove, often in short stretches | Painted | Lacquer starved, board out of line with the applicator |
| Colour mismatch | Bevel colour off the decor, or varying between boards | Painted | Lacquer batch, or a new film lot with the old lacquer shade |
| Gloss line | Bright edge on a matt board | Micro, painted | Milling finish on the wear layer; lacquer gloss |
| Uneven depth or width | Groove wider at one end, or wider on one side of the joint | Micro, painted, pressed | Tool wear, board not square to the tool, press misalignment |
| Chipped edge | Small breaks along the bevel line | All, worst on micro and square edges | Blunt tool, brittle core, handling and packing |
| Misaligned pressed bevel | Pressed groove off the joint line, or uneven between boards | Pressed | Bevel placement in production |
Watch what a depth fault does to a painted bevel. A groove milled deeper than the drawing puts more core in view and asks more of the lacquer, so depth and paint coverage often fail together on the same boards.
How do you tell a bevel fault from a locking fault?
Measure the joint before you judge the bevel. An opening between assembled boards or a height difference across the joint changes how the bevel line looks, and an inspector looking only at the surface will call it a bevel fault. If the joint is closed and flush, the fault is in the bevel; if it is open or stepped, look at the lock and the board geometry first.
The distinction matters because the fix sits in different places. A bevel fault is corrected at the bevel tool, the lacquer unit or the press. An opening at the end joints points to the short-side profile, board length or squareness; a step points to the profile, board thickness or flatness. Those are covered in our guide to SPC click joint testing, including which report proves locking strength.
The table sorts the common symptoms by first suspect.
| Symptom on the test floor | First suspect | How to confirm |
|---|---|---|
| Dark line along the joint, joint closed and flush | Bevel: paint too dark, or groove too deep | Compare a single board’s bevel with the master board |
| Bright line, joint closed | Bevel: gloss line or missed paint | Look at the board alone at a low angle |
| Line wider at one end of a long joint | Board out of square or not straight | Measure squareness and straightness |
| Bright line at the short-end joint, single boards fully painted | Opening at the end joint, showing the unpainted profile | Feeler gauge at the end joint |
| One side of the bevel higher than the other | Height difference across the joint | Straightedge and feeler gauge across the joint |
With no bevel, the last two rows show at once; with a deep painted bevel they can hide for a while. Do not let a deep bevel be the reason a joint fault passes inspection.
Which standards cover the joint line, and which cover the bevel?
None of the standards we checked names the bevel, so its type, dimensions and defect limits are yours to set in the PO. The standards cover the board and joint around it: squareness and straightness of the plank (ISO 24342:2024) and openings and steps between assembled boards (ISO 24337:2019). Both are methods with no pass value; editions and the product standard EN 16511 are set out in the joint testing guide linked above.
Hold-point checks for size and squareness on the first production boards are covered in our SPC production quality control plan.
What should the acceptance rule say?
Put one bevel clause in the specification annex, tied to the drawing and the master board. It names the type and dimensions, the defects counted, how and where boards are viewed, and what counts as a pass. Values in square brackets are yours to agree with the factory.
Bevel. Type: [micro / painted / pressed / none], on [long sides / all four sides], to drawing [number, revision], angle [value] and depth [value] with tolerance [value]. Lacquer (painted bevel only): colour and gloss to master board [ID], checked against each new film lot. Defects counted per board: paint overspill onto face or profile, missed paint or exposed core, colour mismatch to master, gloss line, uneven depth or width, chipped edge, misaligned pressed bevel. Viewing: boards assembled on a test floor from at least [number] pallets, viewed standing at [distance] under [light source], plus single boards at a low angle. Acceptance: [classification of each defect and the limits per sample]. Openings and height differences between assembled boards are judged under the joint clause, measured to ISO 24337:2019. Any change of bevel tool, angle, lacquer supplier or pressing method requires a new sample before shipment.
Two parts of that clause do most of the work. Viewing conditions stop the argument about whether a defect is visible, and the change clause catches a new tool or lacquer brought in after approval. One coating unit’s data sheet lists a central angle adjustment and a colour change for all four sides within 15 minutes, so both are routine on the line.
Where is the bevel checked: sample, line or PSI?
At three points, each answering a different question. The pre-production sample fixes what the bevel should look like. The line check catches tool wear and lacquer drift while boards can still be corrected; if nobody on your side is at the factory, that is where on-line production checks for bevel defects come in. The pre-shipment inspection confirms the packed lot matches the master board.
| Stage | What to check | Evidence to keep |
|---|---|---|
| Pre-production sample | Bevel type, angle and depth against the drawing; lacquer colour and gloss against the decor | Signed master board with bevel noted; drawing revision |
| First production boards | Depth, paint coverage and colour on boards from the new film lot and new tooling | Photos per board ID; depth readings; colour sign-off |
| In line, at each tool or lacquer change | Overspill, coverage, depth | Factory record per tool change, with time and board count |
| Pre-shipment inspection | Defect count on single boards and on a test floor from different pallets | Report with photos of each defect class and the joint measurements |
The in-line row is a factory record you ask for, not a visit you make. Where it sits among the other hold points is covered in the production plan guide linked above. The full inspection method, sampling and defect classes belong to our pre-shipment inspection checklist; the bevel clause is one line in that brief.
Worked example: the bright line at the end joints
Illustrative only. An importer orders a light oak decor with a painted four-sided bevel in a contrasting dark lacquer. At inspection, the test floor shows bright lines at several short-end joints. The first report calls it “bevel paint missing”.
The inspector then measures before judging. On single boards, the dark lacquer covers the bevel on all four sides. On the test floor, a feeler gauge finds an opening at the affected end joints, and the bright line is the unpainted profile below the bevel showing through the opening, not missing paint. Squareness readings on boards from two pallets are outside the agreed limit.
So the fault is board geometry and the short-side lock, not the bevel. The importer asks the factory for the squareness record on the affected run and a joint test on boards from it, keeps the balance on hold, and takes the decision through the options set out in what to do after a failed inspection. Had the report stayed at “bevel paint missing”, the factory would have touched up lacquer on boards whose joints still opened.
Our view
We would never accept “4V bevel” as a specification. The type, angle, depth and lacquer colour go on a drawing, the drawing goes on the master board record, and the change clause covers tool and lacquer. That takes an hour before the deposit and saves the argument at inspection.
On a light decor, we would ask to see a micro-bevelled board at a low angle before approval, because the shiny edge Unilin describes shows most there and is hard to correct on finished boards.
Our pre-shipment inspection service can carry the bevel clause into the inspector’s brief and report each defect class with photos. Related checks before shipment are collected in the shipping and quality guides.
Common mistakes with bevel specifications
Most bevel disputes start with a spec that named the edge but not the defect, or an inspection that looked at boards one at a time. The table lists the ones we would guard against.
| Mistake | What it costs | How to avoid it |
|---|---|---|
| “4V bevel” with no drawing | Factory sets depth and angle; nothing to fail against | Drawing with angle, depth and tolerance, tied to the master board |
| No lacquer colour reference | Bevel shade drifts between lots | Lacquer colour and gloss approved on the master board |
| Judging bevels on single boards only | Joint faults read as bevel faults, or hidden by a deep groove | Test floor from several pallets, joint measured first |
| Deep micro bevel on a thin wear layer | Less wear layer at the edge than contracted | Bevel depth checked against the wear-layer figure |
| New tool or lacquer accepted without a sample | Edge changes after approval | Change clause in the PO |
Questions buyers ask
Can I ask the factory to repaint bevels on boards that fail?
You can ask, but agree first how repainted boards will be checked and kept apart. Touch-up lacquer applied off the line rarely matches the line coat in colour and gloss, so judge repaired boards on a test floor beside untouched ones before accepting them.
What happens if the bevel colour matches the master board but not the decor in a new film lot?
The bevel was approved against one film lot. If the factory changes film lot, the lacquer may need a new shade to match it, so ask for a bevel colour check on the first boards from every new film lot, signed against the master board.
Does a pressed bevel need a patent licence?
Unilin describes its pressed bevel method as patented. If a factory quotes a pressed bevel, ask which method it uses and whether it holds a licence for your market, as you would for a click profile.
Is a bevel defect found after delivery a transit claim?
Almost never. Paint, milling and colour faults are made on the line and show on unopened cartons, so they are a manufacturing claim against the factory. Chipped edges inside crushed cartons are the exception and need packing evidence.
Should the inspector cut boards to check the bevel?
Only to check depth on a pressed or deep painted bevel against the drawing, and only on boards set aside for destructive checks. Paint coverage, colour and chips are judged on whole boards and on the assembled test floor.
Sources & further reading
- Unilin Technologies: Bevel technologies (read November 2026)
- Unilin Technologies: Pressed bevel (read November 2026)
- Unilin Technologies: Matte bevel (read November 2026)
- Kraft Group: Floors, profiling lines incl. chamfer painting (read November 2026)
- Schiele: TransferDisc bevel coating unit, LIGNA 2019 exhibitor data sheet
- ISO 24337:2019, Laminate floor coverings: determination of geometrical characteristics (edition 2, confirmed 2025)
- ISO 24342:2024, Resilient and textile floor coverings: side length, edge straightness and squareness of tiles and planks (edition 4)
Authorship, affiliations & disclosure
Prepared from the technology licensor, equipment makers and ISO catalogue pages listed, read on 11 November 2026. Production methods are as those companies describe them; defect names and the acceptance rule are our method. The worked example is illustrative. We did not inspect or test any product for this guide.
Corrections & editorial informationContinue exploring.
All guides in Shipping & qualitySPC flooring defective container claim: evidence, notice and insurance
Transit damage goes to the carrier or insurer, factory defects to the seller. The evidence file, CISG notice rules and what CIF cover leaves out.
Read the guideFailed SPC pre-shipment inspection: release, rework or reject?
Five options after a failed SPC pre-shipment inspection, a decision tree by defect class, and the PO clauses that decide who pays to re-inspect.
Read the guideSPC container loading inspection photos: what to ask for
A 12-shot list for SPC loading photos, from empty box to seal, each tied to the bill of lading or packing list. Built on the IMO CTU Code.
Read the guide